Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MetalTek MTEK 12% Ni 410 Cast UNS C97300 Nickel-Silver

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 12% Ni 410 Cast UNS C97300 Nickel-Silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTekCast UNS C97300; Cast Grade C97300; Cast ASTM B271, B584; Military MIL-C-15345-7
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
500 kg
Tensile Strength, Ultimate >= 235 MPa
>= 34100 psi
Tensile Strength, Yield >= 120 MPa
>= 17400 psi
Elongation at Break >= 25 %
>= 25 %
Component Elements Properties Metric English Comments
Copper, Cu 65 %
65 %
Lead, Pb 6.0 %
6.0 %
Nickel, Ni 12 %
12 %
Tin, Sn 2.0 %
2.0 %
Zinc, Zn 15 %
15 %
Users viewing this material also viewed the following: