MetalTek MTEK 175 Cast UNS C95400 Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 175 Cast UNS C95400 Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information provided by MetalTekCast UNS C95400; Cast Grade C95400; Cast ASTM B271, B505, B148; AMS 4870 (Centrifugal Casting); Mil QQ-C-390B
Mechanical Properties Metric English Comments
Hardness, Brinell >= 150
>= 150
3000 kg
183
183
3000 kg, typical
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
Elongation at Break >= 12 %
>= 12 %
Component Elements Properties Metric English Comments
Aluminum, Al 11 %
11 %
Copper, Cu 85 %
85 %
Iron, Fe 4.0 %
4.0 %