MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 585 MPa
>= 84800 psi
Tensile Strength, Yield >= 415 MPa
>= 60200 psi
Elongation at Break >= 18 %
>= 18 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.040 %
<= 0.040 %
Carbon, C 0.080 - 0.12 %
0.080 - 0.12 %
Chromium, Cr 8.0 - 9.5 %
8.0 - 9.5 %
Iron, Fe 87.37 - 89.9 %
87.37 - 89.9 %
As Balance
Manganese, Mn 0.30 - 0.60 %
0.30 - 0.60 %
Molybdenum, Mo 0.85 - 1.05 %
0.85 - 1.05 %
Nickel, Ni 0.40 %
0.40 %
Niobium, Nb (Columbium, Cb) 0.060 - 0.10 %
0.060 - 0.10 %
Nitrogen, N 0.030 - 0.070 %
0.030 - 0.070 %
Silicon, Si 0.20 - 0.50 %
0.20 - 0.50 %
Vanadium, V 0.18 - 0.25 %
0.18 - 0.25 %
Descriptive Properties Value Comments
Heat Treatment Normalize & Temper