MetalTek MTEK 430 Martensitic Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Cast Stainless Steel , T 400 Series Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 430 Martensitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 179
179
Tensile Strength, Ultimate >= 485 MPa
>= 70300 psi
Tensile Strength, Yield >= 275 MPa
>= 39900 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 14 - 18 %
14 - 18 %
Iron, Fe 77.88 - 86 %
77.88 - 86 %
As Balance
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 2.0 %
<= 2.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Heat Treatment Anneal