Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Licomer® A 623 Styrene - Acrylate copolymer dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Licomer®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® A 623 Styrene - Acrylate copolymer dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Styrene - Acrylate copolymer dispersionUsage: Licomer® A 623 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. This product provides excellent gloss(wet look), easy buffability with ultra-high-speed machines, excellent water and detergent resistance, excellent removal properties without metal salts, good traffic resistance, low ammonium odor, good dirt repellency and low presence of black heel marks.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Volatiles 59 - 61 %
59 - 61 %
pH 7.0 - 8.0
7.0 - 8.0
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Milky white liquid
Emulsifier Charge Anionic
Solids Type Styrene Acrylate Copolymer
Users viewing this material also viewed the following: