Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Coat
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Water resistant, cold set and hot melt gluable coatingUsage: Michem® Coat 40Y is a versatile water resistant coating. It is gluable with a wide range of water based and hot melt adhesives.Application data: Michem® Coat 40Y can be applied at the corrugator and off-line using either a blade or a rod coater.Michem® Coat is typically used for: Bakery products; Packaged butter; Pizza boxes; Machinery: Electrical components; Metal parts and Sensitive papersFood Contact Information when manufactured in the USA and Belgium:FDA:176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.01 - 1.03 g/cc
1.01 - 1.03 g/cc
pH 9.0 - 10
9.0 - 10
Brookfield Viscosity 250 - 800 cP
250 - 800 cP
Spindle # 3, rpm 60
Viscosity Measurement 20 - 40
20 - 40
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Milky white, semi-viscous liquid
Solids Type Acrylic/Wax