Michelman® Michem® Emulsion 98040M1 Nonionic Fischer Tropsch wax emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 98040M1 Nonionic Fischer Tropsch wax emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic Fischer Tropsch wax emulsionUsage: Michem® Emulsion 98040M1 is an additive used to provide superior slip and antiblock properties. This product is successfully used in paint and varnish applications for these properties as well as abrasion resistance.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in USA: FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 58 - 62 %
58 - 62 %
pH 3.0 - 10
3.0 - 10
2.0 - 12
2.0 - 12
Recommended pH of system
Brookfield Viscosity <= 120 cP
<= 120 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance White, opaque liquid
Emulsifier Charge Nonionic
Solids Type Fischer-Tropsch