Michelman® Michem® In-Line Primer Q4324A Primer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® In-Line Primer
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® In-Line Primer Q4324A Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Michem® In-Line Primer Q4324A is for use with HP Indigo press W7200.Usage: Michem® In-Line Primer Q4324A is designed as a primer for HP Indigo substrates to render them compatible to ink. It can be used on coated paper substrates on the in-line priming unit on the W7200 press.Application Data: Michem® In-Line Primer Q4324A can be applied using the in-line primer unit on the W7200 press. The recommended dry coat weight is 30 to 60 mg/m². Use our Sapphire Indicator Solution to check quality of the coating. The anilox should be kept turning at all times to avoid premature drying of the solution. Cleaning with warm water, IPA or slightly acidic water is recommended.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.02 g/cc
0.980 - 1.02 g/cc
pH 10.8 - 11.2
10.8 - 11.2
Brookfield Viscosity <= 25 cP
<= 25 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Translucent liquid