Michelman® Michem® Lube 743 Nonionic paraffin wax emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Lube
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Lube 743 Nonionic paraffin wax emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic paraffin wax emulsionUsage: Michem® Lube 743 exhibits a high degree of water resistance and excellent compatibility. This product is used in many water based coating applications to increase water resistance and/or surface slip.Compatible with ingredients used in many industries, including: Automotive care products; Building materials; Can and coil coatings; Concrete; Cordage and twine; Deck stains and sealants; Die lubricants; Fiber sizings; Floor polishes; Furniture coatings; Glass; Gloves, balloons, footwear and mechanical seals; Inks; Packaging films; Pressure-sensitive adhesives; Textiles; Urethane foam and VarnishesWhen manufactured in the USA product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted) and Commission Regulation (EU) n° 10/2011(Restricted) Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in the USA: FDA:175.105: Components of adhesives. 175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. 176.180: Components of paper and paperboard in contact with dry foods. Food Contact Information when manufactured with Singapore: FDA:175.105: Components of adhesives. 175.320: Resinous and polymeric components of coatings for polyolefin films.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 67.5 - 68.5 %
67.5 - 68.5 %
pH 6.0 - 7.5
6.0 - 7.5
Brookfield Viscosity <= 150 cP
<= 150 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance White, low viscosity liquid
Emulsifier Charge Nonionic
Solids Type Paraffin