Michelman® Micryl™ 766R Water resistant coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Micryl™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Micryl™ 766R Water resistant coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: General purpose water resistant coatingUsage: Micryl™ 766R is a water and grease resistant coating that can also function as a heat resistant gloss overprint. In such applications, Micryl™ 766R can be applied to paper (non-clay coated), film or foil, either over or under glycol or wax-free inks. This product is gluable with cold set and hot melt glues.Application Data: Micryl™ 766R runs well on a flexo press and can also be applied at the corrugator.Typical uses include: Packaged foods; Preprint; Displays; and SpecialtiesFood Contact Information when manufactured in the USA: FDA: 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.03 - 1.05 g/cc
1.03 - 1.05 g/cc
pH 8.5 - 9.5
8.5 - 9.5
Brookfield Viscosity 100 - 700 cP
100 - 700 cP
Spindle # 3, rpm 60
Viscosity Measurement 20 - 30
20 - 30
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Cream colored, semi-translucent liquid
Solids Type Acrylic