Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 100 cP | 100 cP | @ 100 rpm, #2 |
Parker Chomerics CHO-SHIELD® 4966 Conductive Silicone Coating Conductive Silicone Coating. This is a conductive silver-filled silicone coating. This three-component system is capable of providing 60 dB of shielding effectiveness above 30 MHz. The coating utili.. |
|||
Brookfield Viscosity | 100 - 750 cP | 100 - 750 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4021 SBR Latex ROVENE® 4021 is a “self†cross-linking, carboxylated styrene-butadiene emulsion that has a firm hand with outstanding strength properties. This binder is especially suited for various n.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | #20/200 rpm |
Mallard Creek Polymers ROVENE® 403 Carboxylated Acrylic Copolymer Latex Applications: Rovene® 403 in portland cement mixtures results in increased adhesion to most substrates, improved water resistance, increased flexural strength and good resistance to UV light. Rov.. |
|||
Brookfield Viscosity | 100 - 750 cP | 100 - 750 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4040 SBR Emulsion ROVENE® 4040 is a non-carboxylated styrene-butadiene (SBR) latex emulsion designed for use as a concrete modifier. ROVENE® 4040 is used as a title grout modifier where it enhances adhesion. It.. |
|||
Brookfield Viscosity | 100 - 900 cP | 100 - 900 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4817 SBR Latex ROVENE® 4817 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder is crosslinkable with external crosslinking agents. ROVENE®.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6017 Styrene-Acrylic Emulsion ROVENE® 6017 is a stiff, self-crosslinking styrene-acrylic copolymer emulsion with excellent water resistance and good mechanical stability.APPLICATIONS: ROVENE® 6017 is recommended for bondin.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | #20/200 |
Mallard Creek Polymers Tychem® 3000D Yield Modifier Additive Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | #20/200 rpm |
Mallard Creek Polymers TYLAC® 873 Nitrile Emulsion Tylac® 873 is a carboxylated acrylonitrile-butadiene copolymer latex. Features: good resistance to oil, grease and solvent, compatible with anionic asphalt emulsions, broadens the temperature ran.. |
|||
Brookfield Viscosity | >= 100 cP @Temperature 25.0 °C |
>= 100 cP @Temperature 77.0 °F |
20 RPM, 70% clay/water slip |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 1, rpm 60 |
Michelman® DigiPrime® 4431 Primer Description: Primer for digital printingUsage: DigiPrime® 4431 is a patented flexo and gravure ready coating which provides excellent adhesion of HP Indigo ElectroInks® to a variety of films. .. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 3, rpm 60 |
Michelman® Hydrosize® PA845 Anionic polyamide dispersion Description: Anionic polyamide dispersionUsage: Hydrosize® PA845 is an APE free, aqueous nylon dispersion designed to be used as a fiber sizing in fiber reinforced nylon composites where greater .. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 09625 Cationic ethylene acrylic acid emulsion Description: Cationic ethylene acrylic acid emulsionUsage: Michem® Emulsion 09625 provides excellent chemical resistance. Michem® Emulsion 09625 has proven most useful in floor and other polis.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 09730 Cationic polyethylene emulsion Description: Cationic polyethylene emulsionUsage: Michem® Emulsion 09730 is an additive to improve mar and scratch resistance. This product is used successfully for improving slip and reducing ma.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Emulsion 43240 Polypropylene emulsion Description: Polypropylene emulsionUsage: Michem® Emulsion 43240 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is needed.We .. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Emulsion 66035 Anionic paraffin/polyethylene wax emulsion Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Emulsion 66035 is an excellent waterbeading agent for exterior coatings providing early water beading and anti-blocking prope.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Flex HS-100 Water based heat seal coating Description: Water based heat seal coatingUsage: Michem® Flex HS-100 is a self-priming, low temperature, heat seal coating for plastic films for Flexible Packaging applications. Patent PendingApp.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion Description: Modified ethylene acrylic acid dispersionUsage: Michem®Prime 5931 is a modified ethylene acrylic acid dispersion which provides improved adhesion to polyolefin substrates. It also ex.. |
|||
Brookfield Viscosity | 100 - 700 cP | 100 - 700 cP | Spindle # 3, rpm 60 |
Michelman® Micryl™ 766R Water resistant coating Description: General purpose water resistant coatingUsage: Micryl™ 766R is a water and grease resistant coating that can also function as a heat resistant gloss overprint. In such applications,.. |
|||
Brookfield Viscosity | 100 - 300 cP | 100 - 300 cP | Spindle # 3, rpm 60 |
Michelman® Nomar® 70AFN Non-abrasive paper coating Description: Non-abrasive paper coatingUsage: Nomar® 70AFN is a water based, gluable, non-abrasive coating generally used to provide abrasion protection for gas flushed food packaging or small ap.. |
|||
Brookfield Viscosity | 100 - 400 cP | 100 - 400 cP | Spindle # 2, rpm 60 |
Michelman® VaporCoat® 1500 Description: Water, oil and moisture resistant product for paperUsage: VaporCoat® 1500 is a coating which provides excellent water, oil and grease resistance along with excellent MVTR properties... |
|||
Brookfield Viscosity | 100 - 600 cP | 100 - 600 cP | Spindle # 3, rpm 60 |
Michelman® VaporCoat® 2200R MVTR Description: MVTR, water and grease resistance coatingUsage: VaporCoat® 2200R is a coating which provides water and grease resistance and excellent MVTR properties on kraft liner and other substr.. |
|||
Brookfield Viscosity | 100 - 200 cP @Temperature 20.0 °C |
100 - 200 cP @Temperature 68.0 °F |
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/01 Linear Thermoplastic Polyurethane Elastomer Pearlstick 46-10/01 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a very high thermoplasticity level, available as pellets.Solubility: Pearlstick 46-10/.. |
|||
Brookfield Viscosity | 100 - 1000 cP | 100 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® MaxWhite® 17 Waxable white coating Description: Waxable white coatingUsage: MaxWhite® 17 is a white coating designed to offer excellent brightness before and after wax. This product is both hot melt and cold set gluable. Applicati.. |
|||
Brookfield Viscosity | <= 100 cP | <= 100 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Flex P1853 Water based primer Description: Water based primer for extrusion coated resinsUsage: Michem® Flex P1853 is a primer for metal and paper substrates to promote adhesion to extrusion coated resins resulting in excepti.. |
|||
Brookfield Viscosity | 100 - 700 cP | 100 - 700 cP | Spindle # 3, rpm 60 |
Michelman® SofTak® 126 Non-skid coating Description: Non-skid coating.Usage: SofTak® 126 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather like" feel. This product is .. |
|||
Brookfield Viscosity | 100 - 300 cP | 100 - 300 cP | #2 @ 50 rpm |
Dow Latex XZ 92219.00 Experimental Latex Description: XZ 92219.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as a woven backing latex where a medium sti.. |
|||
Brookfield Viscosity | 100 - 300 cP | 100 - 300 cP | #2 @ 50 rpm |
Dow Latex XZ 92229.03 Experimental Latex Description: XZ 92229.03 is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as adhesive latex for secondary backed tufted carpets. It is a.. |
|||
Brookfield Viscosity | 100 - 400 cP | 100 - 400 cP | RVT (15% in MEK); MQSA 40 A |
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat.. |
|||
Brookfield Viscosity | 100 - 500 cP | 100 - 500 cP | Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/03 Linear Thermoplastic Polyurethane Pearlstick D40-70/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. Sol.. |
|||
Brookfield Viscosity | 100 cP @Temperature 25.0 °C |
100 cP @Temperature 77.0 °F |
|
Loctite® Prism® 4011 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |