Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile

Category Ceramic , Glass , Glass Fiber , Oxide , Silicon Oxide , Other Engineering Material , Composite Fibers
Manufacturer Mid-Mountain Materials
Trade Name SILTEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use where severe temperature conditions exist.SILTEX 36 is manufactured to a finished weight of 36 ounces per square yard. It's heavier weight and tight 12-harness satin weave makes SILTEX 36 the premium product for maximum protection of personnel and equipment against more severe welding splatter, sparks, grinding of metals, etc. SILTEX 36 is also excellent for use in engineered thermal insulation systems that requiring higher strength and improved thermal properties over the lighter-weight materials.The amorphous silica fibers that make up SILTEX are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium.All SILTEX fabrics are available in standard “C” and pre-shrunk (fired) versions, Fabrics are available with several coating/treatment options that enhance certain properties of the product in order to meet required performance characteristics.Information provided by Mid-Mountain Materials.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
Calculated from weight of 36 oz/sy
Thickness 1270 microns
50.0 mil
nom
Thermal Properties Metric English Comments
Melting Point 1700 °C
3100 °F
Maximum Service Temperature, Air 982 °C
1800 °F
Continuous
1260 °C
2300 °F
Intermittent use
Shrinkage 8.00 - 12.0 %

@Temperature 982 °C
8.00 - 12.0 %

@Temperature 1800 °F
Linear
<= 3.00 %

@Temperature 704 °C,
Time 1800 sec
<= 3.00 %

@Temperature 1300 °F,
Time 0.500 hour
Linear
Descriptive Properties Value Comments
Break Strength Min 270 x 180 lb
nom, warp x fill (1" x 4")
Construction Woven fabric, 12 harness satin weave
Material Amorphous Silica 96-99%
Packaging 50 ly per roll or 150 ly master roll
Tolerance 10%
Width, standard 36 in