Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1700 °C | 3090 °F | |
MarkeTech Lithium Aluminum Oxide (LiAlO2) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.4%. |
|||
Melting Point | 1700 °C | 3090 °F | |
Mateck LiAlO2 Substrate single crystals for III-V nitrides |
|||
Melting Point | 1700 °C | 3100 °F | |
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Melting Point | 1700 °C | 3100 °F | |
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Melting Point | <= 1700 °C | <= 3090 °F | |
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET. |
|||
Melting Point | <= 1700 °C | <= 3090 °F | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we.. |
|||
Melting Point | <= 1700 °C | <= 3090 °F | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features.. |
|||
Melting Point | 1700 °C | 3090 °F | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v.. |
|||
Melting Point | <= 1700 °C | <= 3090 °F | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w.. |
|||
Melting Point | 1700 °C | 3092 °F | |
California Fine Wire Alloy 486 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire. |
|||
Melting Point | 1700 °C | 3090 °F | |
ATI Wah Chang TI-3Al-2.5V Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an.. |