Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44HS Moldable

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Mid-Mountain Materials
Trade Name THERMOSEAL® FIBERPAK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44HS Moldable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or spread into thin sections as coating and separating mediums. APPLICATION: THERMOSEAL® FIBERPAK® MOLDABLES are applied with the fingers, towels, spatulas, or from caulking guns. Gloves should be worn when hand applying. THERMOSEAL® FIBERPAK® MOLDABLES are easily formed to any contour or readily pressed into cracks and smoothed out. Water wet the tool to facilitate smoothing and contouring. Drying consists of removing the liquid portion of the mix usually by use of an external heat source at 220-200ºF • 95-150ºC for approximately six hours per inch of thickness.USES: Trough linings for molten metal transferHigh temperature sealing and coatingLight weight refractory shape manufactureTrough coating and patchingFurnace PatchingPACKAGING: 11 oz. Caulking tubes32 oz. Caulking tubesOne Gallon Bucket5 Gallon Buckets55 Gallon DrumsInformation provided by Mid-Mountain Materials.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0382 lb/in³
Fired Density at 2300°F
1.94 g/cc
0.0700 lb/in³
Wet Density
1.11 g/cc

@Temperature 121 °C
0.0399 lb/in³

@Temperature 250 °F
Dry Density
Solids Content 62 %
62 %
Wet
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F
Use Limit
Shrinkage -5.00 %

@Temperature 1260 °C
-5.00 %

@Temperature 2300 °F
Descriptive Properties Value Comments
Alumina 19%
fired
Appearance Sticky Putty
Color White
Description Moldable
Silica 80%
fired