Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.11 g/cc | 0.0401 lb/in³ | method A; ISO 1183:1987 |
Nylacast Impact Nylon 6, Impact Grade Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also.. |
|||
Density | 1.11 - 1.43 g/cc | 0.0401 - 0.0517 lb/in³ | Average value: 1.21 g/cc Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 E Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
Von Roll Isola IMI Varnish 74035 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >99°C. Usa.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPDZ-1000 - 25% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
Loctite® SpeedBonder™ 324 High Impact Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTABLEND CR Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blend for chromium plating, painting and metallizationGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Covestro Bayblend® T50 XF Polycarbonate + ABS Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
Covestro Bayblend® KU 1-1446 Polycarbonate/ABS Blend Good cold impact strength and fuel resistance.Applications: Automotive industry (interior and body parts).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated fr.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Eurotec® Tecotek® BC40 UF45 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, easy flow grade Information provided by Eurotec® |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 745 Nylon 6/69 A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0436G10M20CL Glass/Mineral Reinforced Coupled |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 747 Nylon 6/66 A medium viscosity copolymer. Excellent flexibility and elongation suitable for film and monofilament applications.Data provided by the manufacturer |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® PC/ABS Alloy 304 General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792B |
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, .. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Total Lacqrene® 851 High Impact Polystyrene
(discontinued **) LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg.. |