Mo-Sci Corporation B-40-I Blue Filter Glass

Category Ceramic , Glass , Optical , Filter
Manufacturer Mo-Sci Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mo-Sci Corporation B-40-I Blue Filter Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Lead-free NVIS blue filter glass for incandescent light source.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Thickness 1000 microns
39.4 mil
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C
6.11 µin/in-°F
Transformation Temperature, Tg 407 °C
765 °F
Softening Point 435 °C
815 °F
Dilatometric
Optical Properties Metric English Comments
Refractive Index 1.60
1.60
Transmission, Visible 2.2 %
2.2 %
Photopic, Source 2100 K
UV Transmittance 0.00 %

@Wavelength 580 nm
0.00 %

@Wavelength 580 nm
0.025 %

@Wavelength 380 nm
0.025 %

@Wavelength 380 nm
0.16 %

@Wavelength 480 nm
0.16 %

@Wavelength 480 nm
0.26 %

@Wavelength 440 nm
0.26 %

@Wavelength 440 nm
Descriptive Properties Value Comments
Chromaticity, CIE 1976 0.11
u', Source 2100 K
0.41
v', Source 2100 K
NVIS Radiance 1.7E-11
NR(b), MIL-STD-3009@0.1 fL Luminance, Source 2100 K
9.7E-11
NR(a), MIL-STD-3009@0.1 fL Luminance, Source 2100 K
Tolerance Radius 0.01
r', Source 2100 K