Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres

Category Ceramic , Glass , Oxide , Silicon Oxide
Manufacturer Mo-Sci Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Bulk Density 1.20 g/cc
0.0434 lb/in³
of Dry Beads
Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
pH 7.3
7.3
in water
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature 30.0 - 300 °C
1.78 µin/in-°F

@Temperature 86.0 - 572 °F
Softening Point 830 °C
1530 °F
Component Elements Properties Metric English Comments
Al2O3 2.0 - 5.0 %
2.0 - 5.0 %
Glass
B2O3 10 - 15 %
10 - 15 %
Glass
Copper, Cu 90 - 99 %
90 - 99 %
Coating
Na2O 5.0 - 10 %
5.0 - 10 %
Glass
Nickel, Ni 1.0 - 10 %
1.0 - 10 %
Coating
SiO2 70 - 80 %
70 - 80 %
Glass
Descriptive Properties Value Comments
Approximate Coating Thickness 600-1000 angstroms
Conductivity 0-1% 1/ohm-cm
of pure copper