Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SS4171P model sealer is used to help minimize cure inhibition of addition curing silicone rubber moldmaking material. Properly applied, the model sealer will help to prevent substrates such as sulfur, vinyl, epoxy and soft woods from inhibiting the cure of the silicone rubber moldmaking material. The sealer will allow easy release of the silicone rubber from the model or master.SS4171P should only be used with addition curing products such as the RTV600 series, TSE34XX series, and RTV800 series products. SS4171P sealer should not be used as a model sealer with condensation cure silicone rubber, as it will act as a bonding agent with this product. Condensation cure products include RTV7888 series, RTV42X series, and RTV430 products.SS4171P model sealer can also be applied to addition cured silicone rubber as a parting agent in making two-part molds.It is suggested that a patch test is done before using addition cure silicones. If inhibition is detected, then do a second patch test trying the SS4171P model sealer.Key Performance Properties: Easy application to patternsOne treatment is generally adequate for each wooden patternCan be used on cured addition cured molds GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 0.840 g/cc
0.840 g/cc
at 25°C/4°C
Thermal Properties Metric English Comments
Flash Point -12.0 °C
10.4 °F
Tag open cup
Processing Properties Metric English Comments
Cure Time 30 min
0.5 hour
Approximate
Descriptive Properties Value Comments
Color Blue
Non-Volatile Content 0.14
Users viewing this material also viewed the following: