Cure Time 30 min
0.5 hour
Gwent Electronic Materials D2020823D2 Polymer Dielectric
This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode...
Cure Time 30 min
0.5 hour
Gwent Electronic Materials D2030210D1 Polymer Dielectric
This material is a black colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode..
Cure Time 30 min
0.5 hour
Gwent Electronic Materials D50706D2 Polymer Dielectric
This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode..
Cure Time 30 min
0.5 hour
Gwent Electronic Materials D50706P3 Polymer Dielectric
This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode...
Cure Time 30 - 60 min
0.5 - 1 hour
Gwent Electronic Materials G2020520D1 Gold Metallo-Organic Ink
This is a screen printing ink designed to act as a working electrode when fired onto alumina substrates. This unique MO formulation gives a fired thickness in the order of 0.2 to 0.3 microns. This..
Cure Time 30 min
0.5 hour
Tack-free
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Cure Time 30 min
0.5 hour
Momentive Performance Materials SS4004P Silicone Primer for use with RTV Silicone Adhesive Sealants, Pink
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Cure Time 30 min
0.5 hour
Momentive Performance Materials SS4044P Silicone Primer for use with RTV Silicone Adhesive Sealants, Light Yellow
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Cure Time 30 min
0.5 hour
Momentive Performance Materials SS4120 Silicone Primer for use with RTV Silicone Adhesive Sealants, Clear
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Cure Time 30 min
0.5 hour
Momentive Performance Materials SS4155 Silicone Primer for use with RTV Silicone Adhesive Sealants, Blue
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Cure Time 30 min
0.5 hour
Approximate
Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds
SS4171P model sealer is used to help minimize cure inhibition of addition curing silicone rubber moldmaking material. Properly applied, the model sealer will help to prevent substrates such as sulf..