Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.0481 - 0.0801 g/cc
0.00174 - 0.00289 lb/in³
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D1667
Mechanical Properties Metric English Comments
Tensile Strength >= 0.276 MPa
>= 40.0 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25; ASTM D1056
K Factor (Wear Factor) 0.27
0.27
[BTU]
Compression Set <= 40 %
<= 40 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -40.0 °C
-40.0 °F
Minimum Service Temperature, Air 93.3 °C
200 °F
Descriptive Properties Value Comments
Color Black