Tensile Strength >= 0.276 MPa
>= 40.0 psi
ASTM D3574-75 Test E
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Tensile Strength >= 0.276 MPa
>= 40.0 psi
ASTM D412
Monmouth Rubber & Plastics Durafoamâ„¢ IVN 41 NEO/PVC/NBR
Information provided by Monmouth Rubber & Plastics Corp.