Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.272 g/cc
0.00984 lb/in³
ASTM D1056
Water Absorption <= 5.0 %
<= 5.0 %
Weight change; ASTM D1056
Mechanical Properties Metric English Comments
Tensile Strength >= 1.38 MPa
>= 200 psi
Die A; ASTM D412
Elongation at Break >= 400 %
>= 400 %
Die A; ASTM D412
Compressive Strength 0.0345 - 0.0896 MPa
5.00 - 13.0 psi
Deflection @ 25%; ASTM D1056
Tear Strength 7.01 kN/m
40.0 pli
Die C; ASTM D624
Compression Set <= 25 %
<= 25 %
ASTM D1056
Descriptive Properties Value Comments
Color Black