Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 5.00 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C122A Neoprene/SBR
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C42NBR Nitrile Rubber
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
Deflection @ 25%
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0896 MPa
5.00 - 13.0 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P292HD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Compressive Strength 0.0345 MPa

@Temperature 23.0 °C
5.00 psi

@Temperature 73.4 °F
ASTM D1056
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber
Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons..
Compressive Strength 0.0345 MPa
5.00 psi
Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..
Compressive Strength 0.0345 MPa
5.00 psi
10% deformation
Unifrax Fiberfrax® 440 Ceramic Fiber Paper
440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at o..
Compressive Strength 0.0345 MPa
5.00 psi
25% deformation
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper
The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du..
Compressive Strength 0.0345 MPa
5.00 psi
25% deformation
Unifrax Isofrax® 1260C Paper Fiber
Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l..
Compressive Strength 0.0345 MPa
5.00 psi
10% Compression, Deflection
3M Cushion-Mount™ E1115 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.0345 MPa
5.00 psi
10% Compression, Deflection
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.0345 MPa
5.00 psi
10% Compression, Deflection
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.0345 MPa
5.00 psi
10% Compression, Deflection
3M Cushion-Mount™ 1120 Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.0345 MPa
5.00 psi
10% Compression, Deflection
3M Cushion-Mount™ 1120K Plus Plate Mounting Tape
3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr..
Compressive Strength 0.0345 MPa
5.00 psi
Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
0.25
Monmouth Rubber & Plastics Durafoam™ P291HD EPDM
Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ i..
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
Deflection @ 25%; ASTM D1056-00
Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM
Performance Features: Softness, stiffness & density infinitely variable.High Ozone Resistance. High Ultraviolet Resistance. Non-Staining. Made from Heat Resistant EPDM Non-fogging (plasticizer free..
Copyright © lookpolymers.com All Rights Reserved