Material Notes:
Machinability: Recently amended and revised to reflect a lower maximum lead percentage; C36000 remains the industry standard for general machining and high volume production. The excellent machinability characteristic of C36000 permits full utilization of a screw machine’s capabilities. Workability: Alloy C36000 has a poor capacity to be hot worked. It can be moderately cold worked. However, it is recommended that this be followed by stress relieving at 500 degrees for 1.5 hours to reduce the possibility of stress corrosion cracking. Applications: Free Cutting Brass include general machining and high volume production where the alloy’s excellent machinability can permit full utilization of the screw machine’s capabilities. With the lower maximum lead content, manufacturers are afforded greater latitude in their designs for lead free compliant component and products. Typical applications include plumbing components and products, fittings, adapters, valve stems, and miscellaneous screw machine parts.Information Provided by Mueller Industries Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 72
72
Tensile Strength at Break 386 MPa
56000 psi
Tensile Strength, Yield 310 MPa
45000 psi
Elongation at Break 25 %
25 %
Machinability 100 %
100 %
Component Elements Properties Metric English Comments
Copper, Cu 60 - 63 %
60 - 63 %
Iron, Fe <= 0.35 %
<= 0.35 %
Lead, Pb 2.5 - 3.0 %
2.5 - 3.0 %
Zinc, Zn 33.7 - 37.5 %
33.7 - 37.5 %
Remainder
Processing Properties Metric English Comments
Processing Temperature 260 °C
500 °F
Stress Relieving