Mueller Alloy 3610 Leaded Brass (UNS C36100)

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Mueller Industries Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mueller Alloy 3610 Leaded Brass (UNS C36100).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Mueller Industries Inc.
Component Elements Properties Metric English Comments
Copper, Cu 60 - 63 %
60 - 63 %
Iron, Fe <= 0.35 %
<= 0.35 %
Lead, Pb 3.1 - 3.7 %
3.1 - 3.7 %
Zinc, Zn 35.1 %
35.1 %
Nominal