Multibase Multi-ABS 3522 Utility Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 3522 Utility Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-ABS 3522 utility grade is a black ABS resin produced for wide-specs and recycled resins. This product is suitable for automotive application and for non-critical load bearing parts.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition G) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785-95
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638-95
Elongation at Break 25 %
25 %
ASTM D638-95
Flexural Modulus 2.414 GPa
350.1 ksi
RT; ASTM D-790-95
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256-93a
Optical Properties Metric English Comments
Gloss 30 - 70 %
30 - 70 %
ASTM D2457-90