Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.414 GPa | 350.1 ksi | ASTM D790 |
Lucent Polymers CPP-130 Polypropylene Homopolymer, 30% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | ASTM D790 |
Lucent Polymers CPP-240 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | ASTM D790 |
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | ASTM D790 |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-T30 Homopolymer Polypropylene, 30% Talc Reinforced Information provided by Entec |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | RT; ASTM D-790-95 |
Multibase Multi-ABS 3522 Utility Grade Multi-ABS 3522 utility grade is a black ABS resin produced for wide-specs and recycled resins. This product is suitable for automotive application and for non-critical load bearing parts.Data provid.. |
|||
Flexural Modulus | 2.414 GPa | 350.1 ksi | RT; ASTM D-790-95 |
Multibase Multi-ABS 3525 Clear Data provided by Multibase. |