Material Notes:
This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.892 g/cc
0.892 g/cc
ASTM 792
Melt Flow 100 g/10 min

@Load 2.16 kg,
Temperature 230 °C
100 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 32
32
10 seconds; ASTM D2240
Tensile Strength, Yield 5.83 MPa
845 psi
Elastic; ASTM D412
Elongation at Break 690 %
690 %
Elastic; ASTM D412
Tear Strength 16.7 kN/m
95.0 pli
ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F