Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin
(discontinued **) Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Average value: 235 °C Grade Count:16 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Nozzle Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 249 °C | 455 - 480 °F | |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 - 285 °C | 455 - 545 °F | Injection Molding |
LG Chemical LUPOY HI5002A PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 275 °C | 455 - 527 °F | Injection Molding |
LG Chemical LUPOY SG5009F PC/ABS Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 4107 C Black TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 2599 TPE Thermoplastic Elastomer This material bonds to polypropylene. Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame Retardant Flexibility, GoodHeat StabilizedOzone ResistantPr.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 4001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information pro.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 7011 TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4164 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Nozzle Temperature | 235 - 240 °C | 455 - 464 °F | |
Beijing Chemical Industry KAIFA® HN201-G0 PA6 Resin Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |