Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM 792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
10 seconds; ASTM D2240
Tensile Strength, Yield 5.17 MPa
750 psi
Elastic; ASTM D412
1.21 MPa

@Strain 100 %
175 psi

@Strain 100 %
ASTM D412
Elongation at Break 700 %
700 %
Elastic; ASTM D412
Tear Strength 21.0 kN/m
120 pli
ASTM D624
Compression Set 22 %
22 %
73°F, 70 hours; ASTM D395
75 %
75 %
158°F, 70 hours; ASTM D395
Thermal Properties Metric English Comments
Flame Spread 25 mm/min
1.0 in/min
VSS-302
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F