Multibase Multi-Flex® A 7202 MR TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 7202 MR TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.912 g/cc
0.912 g/cc
ASTM 792
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
ASTM D955
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
10 seconds; ASTM D2240
Tensile Strength, Yield 6.76 MPa
980 psi
Elastic; ASTM D412
Elongation at Break 750 %
750 %
Elastic; ASTM D412
Tear Strength 43.8 kN/m
250 pli
ASTM D624