Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM 792
Melt Flow 6.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
10 seconds; ASTM D2240
Tensile Strength, Yield 3.45 MPa
501 psi
Elastic; ASTM D412
Elongation at Break 300 %
300 %
Elastic; ASTM D412
Flexural Modulus 0.0827 GPa
12.0 ksi
ASTM D790
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Users viewing this material also viewed the following: