Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.11 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.11 g/cc
2.11 g/cc
Mixed; TM R050-16
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
PolyOne Syncure™ V0030G RoHS Polyethylene, Crosslinked (XLPE)
Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.Gel, Torque, and Dispersion were measured on a 100 phr S1025A / 20 phr V0030G Syncure System. Cured for 6 hours..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film
Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film
Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D1505
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 p..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer
Chemraz® 661 perfluoroelastomer is specifically developed by Greene Tweed to meet the unique demands of aggressive plasma systems. This product’s unique formulation provides enhanced plasma..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM 792
Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D792
A. Schulman POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL8575 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe..
Specific Gravity 2.11 - 2.12 g/cc
2.11 - 2.12 g/cc
ASTM D792
Adamas Adalon® 413 PTFE, 20% PPS
Information provided by Adamas, HPM
Copyright © lookpolymers.com All Rights Reserved