Material Notes:
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsTubingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM 792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
10 seconds; ASTM D2240
Tensile Strength, Yield 14.3 MPa
2080 psi
ASTM D638
Elongation at Break 630 %
630 %
ASTM D638
Flexural Yield Strength 13.5 MPa
1960 psi
ASTM D790
Flexural Modulus 0.468 GPa
67.9 ksi
ASTM D790
Tear Strength 92.9 kN/m
530 pli
ASTM D624