Multibase Multi-Flex® TPE A 5010 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 5010 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shoe sole material Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.966 g/cc
0.0349 lb/in³
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
10 sec; ASTM D-2240
Tensile Strength, Ultimate 3.90 MPa
566 psi
ASTM D412
Elongation at Break 870 %
870 %
ASTM D412
Tear Strength 23.7 kN/m
135 pli
ASTM D624