Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 3.90 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.90 MPa
566 psi
ISO 37
Multibase TPSiV® 4100-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Tensile Strength, Ultimate 3.90 MPa
566 psi
ISO 37
Multibase TPSiV® 4200-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Tensile Strength, Ultimate 3.90 MPa
566 psi
ASTM D412
Multibase Multi-Flex® TPE A 4002 DARK GRAY
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 3.90 MPa
566 psi
ASTM D412
Multibase Multi-Flex® TPE A 5010 BLK
Shoe sole material Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 3.90 MPa
566 psi
ASTM D638/D412
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Copyright © lookpolymers.com All Rights Reserved