Material Notes:
The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 2.0 - 5.0 g/10 min
2.0 - 5.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
10 sec; ASTM D-2240
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D412
Elongation at Break >= 700 %
>= 700 %
ASTM D412
Tear Strength >= 30.0 kN/m
>= 171 pli
ASTM D624