Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 6821 BLK This product is based on Kraton G and PP suitable for automotive applications and meets GM, Ford, and Chrysler specifications. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955-89 |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE S906 Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | FRISETTA Test Method |
Nilit RECONYL A H Recycled nylon 6.6 for injection molding Recycled nylon 6.6 for injection molding, heat stabilized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ASTM D955 |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
Kolon KOPA® KN1322VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 6221 C BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Linear Mold Shrinkage | 0.014 - 0.022 cm/cm @Thickness 3.00 mm |
0.014 - 0.022 in/in @Thickness 0.118 in |
ASTM D955 |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | mold average |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Tipco Tipcolene® FPC 40 PPC - 40% Calcium Carbonate Reinforced Polypropylene Copolymer 40% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Applications: AC Blower wheels, parts and appliances.Data provided by Washington Penn Plastic Co., Inc. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ISO 2577 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |
|||
Linear Mold Shrinkage | 0.014 - 0.019 cm/cm | 0.014 - 0.019 in/in | ASTM D955 |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
Eurotec® Tecomid® NB50 NL IT PA 6 super tough Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
E-Polymers TEKAMID® TB120L Lubricated PA6, DAM LubricatedInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM Data; MD |
BASF Ultramid® 8350 HS BK-102 PA6 (Dry) Ultramid 8350 HS BK-102 is a type 6, black pigmented, impact modified graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness
combined with a.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Ashley Polymers Ashlene® 626SB Nylon 6 Copolymer A flexible nylon copolymer, heat stabilized, in black, for tubing and other extrusion applications.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
Tipco Tipcolene® FPT 20 PPC - 20% Talc Reinforced Polypropylene Copolymer Compound 20% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
A. Schulman ComAlloy Comtuf® 164 Polypropylene, Mineral Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |