Multibase Multi-Flex® TPE A 7521 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7521 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ash is 36%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
10 sec; ASTM D-2240
Tensile Strength, Ultimate 6.20 MPa
899 psi
ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
Flexural Modulus 0.0560 GPa
8.12 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 35.0 kN/m
200 pli
ASTM D624