Mechanical Properties Metric English Comments
Flexural Modulus 0.0560 GPa
8.12 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 7521 BLK
Ash is 36%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0560 GPa
8.12 ksi
ISO 178
Chengdu Polyster H2040 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Like H4040, except that heat-ageing resistance is improved. Applications requiring better heat-ageing resistanc..