Multibase Multi-Flex® TPE A 8299 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8299 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 30 g/10 min
30 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
10 sec; ASTM D-2240
Tensile Strength, Ultimate 4.00 MPa
580 psi
ASTM D412
Elongation at Break >= 150 %
>= 150 %
ASTM D638
Flexural Modulus 0.0700 - 0.150 GPa
10.2 - 21.8 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 30.5 kN/m
174 pli
ASTM D624