Multibase Multi-Flex® TPE D 5303 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE D 5303 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0106 cm/cm
0.0106 in/in
ASTM D955
Melt Flow 0.79 g/10 min
0.79 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
10 sec; ASTM D-2240
Tensile Strength, Ultimate 16.7 MPa
2420 psi
ASTM D412
Elongation at Break 557 %
557 %
ASTM D412
Flexural Modulus 0.438 GPa
63.5 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 139.7 kN/m
797.1 pli
ASTM D624