Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE D 5303 BLK Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D792 |
Polymer Industries Densetec PP Copolymer Sheet Polymer Industries’ Densetec Copolymer Propylene differs from the Densetec Homopolymer Polypropylene by virtue of an additional monomer in the product, thus making it a copolymer material. This is .. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
M. Holland Company CP501 Polypropylene Impact Copolymer AntistaticImpact copolymerHigh flowGood impact resistanceNucleatedGood stiffnessApplications: FurnitureHousehold goodsOutdoor furnishingsToys |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
M. Holland Company CP710 Polypropylene Impact Copolymer AntistaticImpact copolymerGood flowGood impact resistanceNucleatedApplications: ClosuresHousehold goodsThin-walled parts |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
M. Holland Company RP400 Polypropylene Random Copolymer AntistaticHigh clarityRandom copolymerApplications: Food containersHousehold goodsPackaging |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Flint Hills P9H8M-015 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Flint Hills P9H9Z-018 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D792 |
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP) Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of .. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Bapolene® 4071 Polypropylene, Fiber/Injection Grade Bapolene PP4071 is a high flow PP homopolymer for staple and continuous filament applications as well as general purpose injection molding. This resin exhibits good melt and thermal stability.Appli.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |