Material Notes:
Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactured by Shell, under the reference Kraton G 7155 and complies to the internal specifications of Shell/Multibase. The burn rate is 0.99 in/min (24.8 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 4.2 g/10 min
4.2 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
10 sec; ASTM D-2240
Tensile Strength, Ultimate 5.20 MPa
754 psi
ASTM D412
Elongation at Break 217 %
217 %
ASTM D412
Flexural Strength 6.10 MPa
885 psi
Flexural Modulus 0.217 GPa
31.5 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 31.5 kN/m
180 pli
ASTM D624
Users viewing this material also viewed the following: