Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE G 7150 BLK Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Premix Thermoplastics PRESEAL® TPE 6070 PRESEAL TPE 6070 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Premix Thermoplastics PRESEAL® TPE 6071 PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |
|||
Density | 1.85 g/cc | 0.0670 lb/in³ | |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs... |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC
(discontinued **) QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It of.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Haveg 41N Phenolic; Silicate Reinforced Ablative Material A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for abla.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Z25 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Z60 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |
|||
Density | 1.85 g/cc @Temperature 25.0 °C |
0.0668 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Keldax® 6705B Filled Thermoplastic Ethylene Polymer A filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailability: Nor.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | Relative Density; ISO 1183 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | DIN 53479 |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GF45 NL PBT 45% filled, high gloss, increased density Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |
|||
Density | 1.85 g/cc @Thickness >=0.000 mm |
0.0668 lb/in³ @Thickness >=0.000 in |
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3 |
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relati.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65 Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.85 - 1.95 g/cc | 0.0668 - 0.0704 lb/in³ | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.85 - 2.05 g/cc | 0.0668 - 0.0741 lb/in³ | Molded |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |