Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO 1047-3000

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO 1047-3000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955-95
Melt Flow 1.8 g/10 min
1.8 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 12.3 MPa
1780 psi
ASTM D638-95
Elongation at Break 570 %
570 %
ASTM D638-95
Elongation at Yield >= 23 %
>= 23 %
ASTM D638-95
Flexural Modulus 0.257 GPa
37.3 ksi
Secant 1%; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Tear Strength 98.0 kN/m
559 pli
ASTM D624-95
Users viewing this material also viewed the following: