Material Notes:
Multi-Flex® D 5303 is a TOP compound for automotive applications such as bumper covers and side panels.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792-91
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 17.9 MPa
2600 psi
20" / min.; ASTM D-683-95
Elongation at Break 260 %
260 %
ASTM D638-95
Flexural Modulus 1.021 GPa
148.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact 20.9 J
15.4 ft-lb
ASTM D5420