Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM 792
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
10 seconds; ASTM D2240
60
60
ASTM D2240
Tensile Strength at Break 3.79 MPa
550 psi
Elastic; ASTM D412
Tensile Strength, Yield 0.931 MPa

@Strain 300 %
135 psi

@Strain 300 %
ASTM D412
2.00 MPa

@Strain 100 %
290 psi

@Strain 100 %
ASTM D412
Elongation at Break 630 %
630 %
Elastic; ASTM D412
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F