Material Notes:
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
0.610 g/cc
0.0220 lb/in³
Typical; unexpanded product
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Two stage pre-expansion; Usual Use