Physical Properties Metric English Comments
Density 0.0100 - 0.0250 g/cc
0.000361 - 0.000903 lb/in³
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
Density >= 0.0100 g/cc
>= 0.000361 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant
b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 65D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Two stage pre-expansion; Usual Use
NOVA Chemicals Gedexcel® 65L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plasters with low thermal conductivity.Information provided by NOVA Chemicals...
Density >= 0.0100 g/cc
>= 0.000361 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Polimeri Europa Extir® LN 7000 Expandable Polystyrene
Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e..
Density 0.0100 - 0.0250 g/cc
0.000361 - 0.000903 lb/in³
Density range normally used
Polimeri Europa Extir® A 5000 Expandable Polystyrene, Standard  (discontinued **)
Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type A..
Density 0.0100 - 0.0150 g/cc
0.000361 - 0.000542 lb/in³
Density range normally used
Polimeri Europa Extir® A 7000 Expandable Polystyrene, Standard  (discontinued **)
Particle size range is 1.5 - 2.2 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type A..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® IA 7000 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 1.4 - 2.2 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type I..
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova T443B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Density <= 0.0100 g/cc
<= 0.000361 lb/in³
TMA
Akzo Nobel Expancel® 009 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1702 100 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1710 100 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1710 120 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1710 50 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1710 60 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1712 100 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 g/cc
0.000361 lb/in³
ISO 845
BASF Neopolen® P 9270 0.1 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..
Density 0.0100 - 0.100 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.00361 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® 1710 40 mm Expanded Polyethylene
Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF
Density 0.0100 - 0.0200 g/cc
0.000361 - 0.000723 lb/in³
Density range normally used
Polimeri Europa Extir® IA 5000 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.8 - 1.5 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l.Processing technology used for Type I..
Density 0.0100 - 0.400 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.0145 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe)
Description: Neopolen® P 92HD 105 is expanded Polypropylene supplied in the form of beads. The cells are largely closedInformation provided by BASF